Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Multibase Nylex™ 4032 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Flexural Strength | 62.1 MPa | 9010 psi | ASTM D790 |
PolyOne Maxxam™ DP-8463-7001 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-10GB/15KV Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledAramid Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 62.1 MPa | 9010 psi | ASTM D790 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 62.1 MPa | 9010 psi | Type I, 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ecomass® 1003TU96 Tungsten Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Ensinger Tecatron® XP-88 Compression Molded PPS Compound, with 10% Graphite, 15% PTFE and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |
|||
Flexural Strength | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Flexural Strength | 62.1 - 89.6 MPa | 9000 - 13000 psi | |
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC. |
|||
Flexural Strength | 62.1 MPa | 9010 psi | ASTM D790 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Flexural Strength | >= 62.1 MPa | >= 9000 psi | |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated
(discontinued Description/Features:Glass Bead FilledPTFE/Silicone LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 62.1 MPa | 9000 psi | ASTM D790 |
PolyOne Stat-Tech™ AT-000/000 ESD Acetal-Copolymer
(discontinued **) Description/Features:AntistaticInformation provided by PolyOne Corporation. |