Material Notes:
NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical characteristics, high impact strength, and lower thermal expansion. Typical applications include wheels, rollers, bearings & bushings, gears, and valve seals.Data provided by the manufacturer, Cast Nylons Limited.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
24 hrs; ASTM D570
Water Absorption at Saturation 0.66 %
0.66 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength 54.5 MPa
7900 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Tensile Modulus 1.59 GPa
230 ksi
ASTM D638
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 1.64 GPa
238 ksi
ASTM D790
Compressive Strength 68.9 MPa
10000 psi
ASTM D695
Compressive Modulus 1.54 GPa
224 ksi
ASTM D695
Shear Strength 42.1 MPa
6100 psi
ASTM D732
Izod Impact, Notched 1.61 J/cm
3.02 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.2 - 0.3
0.2 - 0.3
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C
55.0 µin/in-°F
ASTM D696
Melting Point 177 °C
351 °F
ASTM D789
Maximum Service Temperature, Air 121 °C
250 °F
Continuous
149 °C
300 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60.0 Hz
3.7

@Frequency 60.0 Hz
ASTM D150
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
ASTM D150
3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 19.7 - 23.6 kV/mm
500 - 600 kV/in
ASTM D149