Multibase Nylex™ 4032 Polyamide + PP

Category Polymer , Thermoplastic , Nylon , Polypropylene (PP)
Manufacturer Multibase
Trade Name Nylex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Nylex™ 4032 Polyamide + PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM 792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
73°F; ASTM D256
Gardner Impact 2.825 J
2.083 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Unannealed; ASTM D648
Vicat Softening Point 175 °C
347 °F
ASTM D1525
Flammability, UL94 HB
HB