Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Flexural Strength | <= 46.0 MPa | <= 6670 psi | ISO 178 |
Polykemi AB POLYfill PP HIP16020FCF Polypropylene, Fast Cycle Information provided by Polykemi AB |
|||
Flexural Strength | <= 46.0 MPa | <= 6670 psi | ISO 178 |
Polykemi AB POLYfill PPC T20040 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 46.0 MPa | <= 6670 psi | ISO 178 |
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 46.0 MPa | <= 6670 psi | ISO 178 |
Polykemi AB POLYfill PPH TS4020D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer
(discontinued **) Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | at 3.5% strain; ISO 178 |
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ML003 PP (Europe-Africa-Middle East) LNP* Lubricomp* ML003 is a compound based on Polypropylene resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ISO 178 |
Styrolution PS 416N HIPS Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | cond; ISO 178 |
DSM Novamid® 1010N2 1ES NAT PA6 FR(30) Injection Molding, Flame Retardant (Halogen free) |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Entec Hypro™ PPC-T40 Copolymer Polypropylene, 40% Talc Reinforced Information provided by Entec |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 HI2 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | XY direction; ASTM D790 |
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 164 Polypropylene, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436G10M20CL Glass/Mineral Reinforced Coupled |
|||
Flexural Strength | 46.0 MPa | 6670 psi | |
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Flexural Strength | <= 46.0 MPa | <= 6670 psi | ISO 178 |
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 46.0 MPa | <= 6670 psi | ISO 178 |
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ASTM D790 |
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
Flexural Strength | 46.0 MPa | 6670 psi | ISO 178 |
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled Heat stabilizedInformation provided by PolyPlastic Group. |