Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON AX01706 ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON AX01706 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Moisture Absorption 0.190 %
0.190 %
50% RH, 24 hrs; ASTM D570
0.270 %
0.270 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.0 MPa
3480 psi
5 mm/min; ISO 527
27.0 MPa
3920 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 28.0 MPa
4060 psi
5 mm/min; ISO 527
30.0 MPa
4350 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 5.8 %
5.8 %
Type I, 5 mm/min; ASTM D638
7.4 %
7.4 %
5 mm/min; ISO 527
Elongation at Yield 1.8 %
1.8 %
5 mm/min; ISO 527
1.9 %
1.9 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.03 GPa
294 ksi
1 mm/min; ISO 527
2.04 GPa
296 ksi
50 mm/min; ASTM D638
Flexural Strength 46.0 MPa
6670 psi
1.3 mm/min, 50 mm span; ASTM D790
52.0 MPa
7540 psi
ISO 178
Flexural Yield Strength 52.0 MPa
7540 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.03 GPa
294 ksi
2 mm/min; ISO 178
2.07 GPa
300 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.73 J/cm
8.86 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 3.00 J
2.21 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
96.0 °C

@Thickness 3.20 mm
205 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
88.0 °C

@Thickness 3.20 mm
190 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257