Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 112 MPa | 16200 psi | |
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Flexural Strength | 112 MPa | 16200 psi | |
Poco Graphite ZXF-5Q Industrial Grade Graphite SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D790 |
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D 790 |
NOVA Chemicals Dylark® FG7200 High-Heat Styrenic Copolymer Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Flexural Strength | 112 MPa | 16200 psi | 2mm/min; ASTM D790 |
Kingfa JH720 G10 10% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanner cabinetComputer plug partsCD-ROM, DVDElectri.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 112 MPa @Strain 3.50 %, Temperature 175 °C |
16200 psi @Strain 3.50 %, Temperature 347 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Flexural Strength | 112 MPa | 16200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 0177 B Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac.. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Techmer ES Luriblend® PA6 ML3 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(3%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Black.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D 790 |
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Strength | 112 MPa | 16200 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D790 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Flexural Strength | 112 MPa | 16200 psi | dry; ISO 178 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D790 |
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin.. |
|||
Flexural Strength | >= 112 MPa | >= 16200 psi | cold bending |
China-Yixing Longly Refractories Push Slab Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Flexural Strength | 112 MPa | 16300 psi | ASTM D790 |
Asahi Kasei Thermylene® P-25FG-3809 25% Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Flexural Strength | 112 MPa @Temperature 120 °C |
16200 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Strength | 112 MPa | 16200 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 249 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 112 MPa @Temperature 175 °C |
16200 psi @Temperature 347 °F |
3.5% Strain; ISO 178 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |