Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 105 MPa | 15200 psi | ASTM D790 |
Plaskolite Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Flexural Strength | 105 MPa | 15200 psi | ASTM D790 |
Plaskolite West Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Flexural Strength | 105 MPa | 15200 psi | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Flexural Strength | <= 105 MPa | <= 15200 psi | ISO 178 |
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Strength | <= 105 MPa | <= 15200 psi | ISO 178 |
Polykemi AB SCANTEC PC S85R V0 Polycarbonate, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Strength | 105 MPa | 15200 psi | |
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Flexural Strength | 105 MPa | 15200 psi | ASTM D790 |
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Flexural Strength | 105 MPa | 15200 psi | 3.5%; ISO 178 |
GEHR Plastics PMMA Acrylic Polymethylmethacrylate is refractory and shows a good mechanical strength, tensile strength and hardness. PMMA is also scratch resistant and easy to polish. It shows good temperature resistance and .. |
|||
Flexural Strength | 105 MPa | 15200 psi | 1.5 mm/min; ISO 178:2001 |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Flexural Strength | 105 MPa | 15200 psi | 1.5 mm/min; ISO 178:2001 |
Global EPP PA 6C WFN Cast Polyamide 6 + Wax Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Flexural Strength | 105 MPa | 15200 psi | 2 mm/min; ISO 178 |
Lucite International Perspexâ„¢ GS IM Acrylic Cast Sheet OM14 PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me.. |
|||
Flexural Strength | 105 MPa | 15200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Flexural Strength | 105 MPa | 15300 psi | ASTM D790 |
Techmer ES HiFill® ABS GF10 LE 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 105 MPa | 15200 psi | ASTM D790 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Flexural Strength | 105 MPa | 15200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Strength | 105 MPa | 15200 psi | ISO Data |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Flexural Strength | 105 MPa | 15200 psi | ASTM D790 |
Saint-Gobain Meldin® 7001 Isostatically Molded Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Flexural Strength | 105 MPa | 15200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Flexural Strength | 105 MPa | 15200 psi | D790 |
Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Flexural Strength | 105 MPa | 15300 psi | ASTM D790 |
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 105 MPa | 15200 psi | ISO 178 |
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
Flexural Strength | 105 MPa | 15200 psi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 640Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Flexural Strength | 105 MPa | 15200 psi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Flexural Strength | 105 MPa | 15200 psi | ASTM D-790 |
Plaskolite West Optix® CA - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 105 MPa | 15200 psi | ASTM D790 |
Beijing Chemical Industry KAIFA® MN-401 PA6 Resin Good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Strength | 105 MPa | 15200 psi | 2mm/min; 80x10x4mm; ISO 178 |
SYNTHOS Krasten® 171 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high .. |