Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, PTFE-Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Filler Content 25 %
25 %
Water Absorption 0.040 %

@Time 86400 sec
0.040 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 117
117
ASTM D785
Tensile Strength 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 5.6 %
5.6 %
ASTM D638
5.7 %
5.7 %
Flexural Strain; ASTM D790
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Flexural Strength 105 MPa
15300 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Compressive Strength 110 MPa
16000 psi
ASTM D695
Compressive Modulus 2.34 GPa
340 ksi
ASTM D695
Izod Impact, Notched 0.315 J/cm
0.590 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+13 ohm
<= 1.00e+13 ohm
ASTM D257
Descriptive Properties Value Comments
Color Tan