Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.40 MPa @Strain 10.0 %, Temperature 23.0 °C |
1220 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**) Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,.. |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.40 MPa @Strain 100 % |
1220 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
Tensile Stress | 8.40 MPa @Strain 10.0 % |
1220 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM460-H TPC-ET Injection Molding, Heat Stabilized |
|||
Tensile Stress | 8.40 MPa @Strain 50.0 % |
1220 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.42 MPa @Strain 54.54 %, Temperature 40.0 °C |
1220 psi @Strain 54.54 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.38 MPa @Strain 37.22 %, Temperature 120 °C |
1220 psi @Strain 37.22 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.40 MPa @Strain 47.19 %, Temperature 120 °C |
1220 psi @Strain 47.19 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.41 MPa @Strain 134.13 %, Temperature 120 °C |
1220 psi @Strain 134.13 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.40 MPa @Strain 5.68 %, Time 36000 sec |
1220 psi @Strain 5.68 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 8.40 MPa @Strain 6.81 %, Time 3.60e+6 sec |
1220 psi @Strain 6.81 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 8.40 MPa @Time 3600 sec, Strain 4.98 % |
1220 psi @Time 1.00 hour, Strain 4.98 % |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 8.40 MPa @Strain 6.32 %, Time 360000 sec |
1220 psi @Strain 6.32 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 8.40 MPa @Strain 7.26 %, Time 3.60e+7 sec |
1220 psi @Strain 7.26 %, Time 10000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 8.44 MPa @Strain 0.400 %, Temperature 60.0 °C |
1220 psi @Strain 0.400 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 8.40 MPa @Strain 0.0400 %, Temperature 40.0 °C |
1220 psi @Strain 0.0400 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 8.42 MPa @Strain 0.310 %, Temperature -20.0 °C |
1220 psi @Strain 0.310 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 8.38 MPa @Strain 0.0400 %, Temperature 23.0 °C |
1220 psi @Strain 0.0400 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 8.44 MPa @Strain 0.180 %, Temperature 90.0 °C |
1220 psi @Strain 0.180 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |
|||
Tensile Stress | 8.40 MPa @Strain 50.0 % |
1220 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.40 MPa @Strain 10.0 % |
1220 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 8.41 MPa @Strain 100 % |
1220 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |