Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific) AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP4 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -17.8 °C |
5.00 ft-lb/in @Temperature 0.000 °F |
ASTM D256 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm |
5.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm |
5.00 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 7000 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS GN005 Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX1701 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Formosa Plastics Formolene® 2306N Impact Copolymer Polypropylene Impact Copolymer for Compression and Injection Molded Caps and Closures Formolene® 2306N is a polypropylene copolymer formulated for compression and injection molded cap applications. It was create.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm |
5.00 ft-lb/in @Thickness 0.250 in |
|
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm |
5.00 ft-lb/in @Thickness 0.250 in |
|
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 0.000 °C |
5.00 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
5.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 7456 Rigid PVC, Extrusion Georgia Gulf 7456 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessWeatherabilityWeldabilityChemical ResistanceEase of Proces.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -20.0 °C |
5.00 ft-lb/in @Temperature -4.00 °F |
ASTM D-256 |
Axiall SP-7008 Rigid PVC, Molding Georgia Gulf SP-7008 is a rigid vinyl compound formulated for electrical fittings and molded parts requiring high impact strength and toughness.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D-256 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 6.35 mm |
5.00 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall ProTherm® 4345 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties .. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 922 NAT Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS SLX2 MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |