Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | shear, Al/Al |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | |
Whitecast Polymer Engineering Epoxy Composite Casting Whitecast Polymer Engineering (WPE) low-density material is used for acoustic dampening requirements (Damping ratio = 0.158). There is an order of magnitude higher vibration dampening realized when.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F199 High Temperature Anaerobic Adhesive System TRA-BOND F199 is a high strength, anaerobic adhesive for fiberoptic terminations. Although specifically designed for bonding glass and plastic fiber to plastic ferrules, it also bonds exceptionally .. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond FDA16 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-16 EPOXY ADHESIVE is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests,.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond GA47-2LV Instrument Adhesive TRA-BOND GA47-2LV low viscosity adhesive is designed for guidance instrument applications. This adhesive exhibits excellent compatibility with conventional gyro flotation fluids. TRA-BOND GA47-2LV a.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum, @ 125°C |
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are r.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive Ablebond 862-2 room temperature curing epoxy adhesive is designed for solder pad encapsulation or sealing the head/disk area in floppy disc assemblies. This resilient compound is suitable for bondin.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond GA47-2LVU Low Viscosity Instrument Adhesive TRA-BOND GA47-2LVU is a low viscosity adhesive designed for guidance instrument applications. This adhesive exhibits excellent compatibility with conventional gyro flotation fluids.Information provi.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-30CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | ASTM D4541 |
Chesterton ARC S1 General purpose coating Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | ASTM D4541 |
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | Tensile; ASTM D4541 |
Chesterton MRS S4+ Metal Rebuilding System An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 .. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Brushable Ceramic - White Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-309 Low Expansion Epoxy Adhesive EB-309 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional .. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-348 Low Expansion Epoxy Adhesive EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional .. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Al-to-Al Lap Shear; Cured property; ASTM D1002 |
Aptek 6505PMF Electronic-grade, non-conductive adhesive APTEK 6506-PMF is a one component, 100% solid, mineral-filled epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards as well as a protective barri.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-00CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-00NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-05CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 13.8 - 15.9 MPa @Temperature -55.0 - 93.0 °C |
2000 - 2310 psi @Temperature -67.0 - 199 °F |
Average value: 14.9 MPa Grade Count:1 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |