Material Notes:
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.Loctite® E-00NS Non-sag, controlled flow, low odor Durabond® Epoxy AdhesiveA non-sag epoxy with a 5-minute worklife. Translucent, controlled flow, low odor.Mix Ratio by Volume, Resin:Hardener = 1:1 Bonding Type: Epoxy
Physical Properties Metric English Comments
Viscosity 375000 cP
375000 cP
Mixed - high; Resin - 375,000 cP; Hardener - 375,000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Adhesive Bond Strength 13.8 - 27.6 MPa
2000 - 4000 psi
Varies with substrates
Peel Strength 0.175 - 0.877 kN/m
1.00 - 5.00 pli
Varies with substrates.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Test run on 1/8" specimens.
Processing Properties Metric English Comments
Pot Life 3.0 - 5.0 min
3.0 - 5.0 min
Descriptive Properties Value Comments
Color Translucent