Material Notes:
EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional stability and excellent chemical resistance.Information provided by Epoxyset Inc.
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
Water Absorption 0.20 %
0.20 %
Viscosity >= 40000 cP
>= 40000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 93
93
ASTM D2240
Adhesive Bond Strength 13.8 MPa
2000 psi
Lap Shear Strength
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C
12.8 µin/in-°F
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 93.0 °C
199 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
60.0 min

@Temperature 100 °C
1.00 hour

@Temperature 212 °F
Pot Life 120 min