Material Notes:
Whitecast Polymer Engineering (WPE) low-density material is used for acoustic dampening requirements (Damping ratio = 0.158). There is an order of magnitude higher vibration dampening realized when using WPE composite rather than aluminum and steel. WPE material is 3-5 times greater in vibration dampening than granite.The product has excellent chemical resistance. The aggregate filler blend has been designed for optimum compressive modulus. The purity of the aggregate, particle shape, particle size and particle size distribution are the factors considered during the development of the WPE aggregate material. Combining these materials has resulted in the most stable material used in the polymer composite industry.Information provided by Whitecast Polymer Engineering.
Physical Properties Metric English Comments
Density 2.35 g/cc
0.0851 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 91
91
Tensile Strength, Ultimate 14.5 MPa
2100 psi
Modulus of Elasticity 31.0 GPa
4500 ksi
Compressive Strength 162 MPa
23500 psi
Adhesive Bond Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
CTE, linear 16.9 µm/m-°C

@Temperature 20.0 °C
9.40 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -45.6 °C
-50.0 °F
Descriptive Properties Value Comments
Damping Ratio 0.158