Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Grit Blasted Steel, Shear; ASTM D1002 |
Permabond 935 Cyanoacrylate The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | tensile shear; ASTM D1002 |
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue Information provided by ITW Devcon |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | shear, Al/Al |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | |
Whitecast Polymer Engineering Epoxy Composite Casting Whitecast Polymer Engineering (WPE) low-density material is used for acoustic dampening requirements (Damping ratio = 0.158). There is an order of magnitude higher vibration dampening realized when.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 9059D Rigid Unfilled Epoxy Adhesive TRA-BOND 9059D rigid, unfilled epoxy adhesive exhibits good dimensional stability for gyro applications. This material is a blue-green color.Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F199 High Temperature Anaerobic Adhesive System TRA-BOND F199 is a high strength, anaerobic adhesive for fiberoptic terminations. Although specifically designed for bonding glass and plastic fiber to plastic ferrules, it also bonds exceptionally .. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum, @ 125°C |
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are r.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive Ablebond 862-2 room temperature curing epoxy adhesive is designed for solder pad encapsulation or sealing the head/disk area in floppy disc assemblies. This resilient compound is suitable for bondin.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | |
Trelleborg Emerson & Cuming Eccobond® C429-2 One-Component Silver Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming C429-2 Eccobond® One-Component Silver Filled Electrically Conductive Epoxy AdhesiveOne component, high strength, moderate cost, silver filled, electrically conductive, epoxy adhesi.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-20NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-30CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | ASTM D4541 |
Chesterton ARC MXHT High temperature severe wear compound Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | ASTM D4541 |
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon High-Performance Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Sprayable Ceramic™ Epoxy Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-348 Low Expansion Epoxy Adhesive EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional .. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | ASTM D4541 |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Al-to-Al Lap Shear; Cured property; ASTM D1002; 50 grit, sanded/solvent wiped |
Aptek 2201-A/B Fast set urethane adhesive APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving f.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-00CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Varies with substrates |
Loctite® Durabond® E-00NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 13.8 - 15.9 MPa @Temperature -55.0 - 93.0 °C |
2000 - 2310 psi @Temperature -67.0 - 199 °F |
Average value: 14.9 MPa Grade Count:1 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Adhesive Bond Strength | 13.8 MPa | 2000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Adhesive Bond Strength | >= 13.8 MPa | >= 2000 psi | Metal; ASTM D4541 |
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater si.. |