Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Poco Graphite AXZ-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Modulus of Elasticity | 9.00 - 11.0 GPa | 1310 - 1600 ksi | Injection; ISO 527 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Modulus of Elasticity | 9.00 - 10.0 GPa | 1310 - 1450 ksi | Injection; ISO 527 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Modulus of Elasticity | 9.00 - 11.0 GPa | 1310 - 1600 ksi | Compression and Injection; ISO 527 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Modulus of Elasticity | 9.00 - 11.0 GPa | 1310 - 1600 ksi | Compression; ISO 527 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Modulus of Elasticity | 9.00 - 11.0 GPa | 1310 - 1600 ksi | Injection and Compression; ISO 527 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Modulus of Elasticity | 9.00 - 11.0 GPa | 1310 - 1600 ksi | Average value: 10.1 GPa Grade Count:6 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 9.00 - 18.6 GPa | 1310 - 2700 ksi | Average value: 14.0 GPa Grade Count:26 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 1-8064 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 20-8332 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/10/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 50/CF/7/GF/20/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 50-7110 Polycarbonate, with carbon fiber, low-warpage, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Electrically conductive, suitable for continuous discharging o.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 50-7154/V0 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | |
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527-2 |
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 9.00 GPa @Thickness >=1.50 mm |
1310 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527 |
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Modulus of Elasticity | 9.00 GPa @Temperature 80.0 °C |
1310 ksi @Temperature 176 °F |
ISO 527 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Modulus of Elasticity | 9.00 - 11.0 GPa | 1310 - 1600 ksi | Injection; ISO 527 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527-1/-2 |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Conditioned) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |