BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F], for instance, for automotive plug-in connectors.Information provided by BASF
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Moisture Absorption at Equilibrium >= 0.80 %
>= 0.80 %
50% RH; ISO 62
>= 4.5 %
>= 4.5 %
Saturation; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
ISO 527
235 MPa

@Temperature -40.0 °C
34100 psi

@Temperature -40.0 °F
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Modulus of Elasticity 9.00 GPa
1310 ksi
ISO 527-1/-2
Charpy Impact Unnotched 10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Melting Point 295 °C
563 °F
DIN 53765
Decomposition Temperature >= 350 °C
>= 662 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Dielectric Constant 4.5

@Frequency 1.00 Hz
4.5

@Frequency 1.00 Hz
IEC 60250
Dissipation Factor 0.040

@Frequency 1.00e+6 Hz
0.040

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 80.0 °C
176 °F
Hopper Throat
Zone 1 300 °C
572 °F
Feed Zone
Zone 2 310 °C
590 °F
Compression
Zone 3 320 °C
608 °F
Metering-zone
Zone 4 320 °C
608 °F
Nozzle
Descriptive Properties Value Comments
Color BK 00564
Commercial Status North America
Peripheral screw speed <0.3 m/s