Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.50 - 8.00 GPa | 798 - 1160 ksi | Average value: 7.05 GPa Grade Count:6 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 5.50 - 31.8 GPa | 798 - 4610 ksi | Average value: 14.3 GPa Grade Count:46 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | Storage |
Lord Adhesives Thermosetâ„¢ ME-541 Underfill Encapsulant LORD Thermosetâ„¢ ME-541 encapsulant is an anhydride free, high purity, semi-conductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip chip devi.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 1-0866 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-2 |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-2 |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-2 |
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO R527 |
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | Conditioned; ISO 178 |
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-2 |
BASF Ultradur® S 4090 GX 14% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-2 |
BASF Ultradur® B 4406 G2 10% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 178 |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 178 |
Addiplast Addinyl C2 ZV15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 5.50 - 12.4 GPa | 798 - 1800 ksi | Average value: 10.4 GPa Grade Count:21 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/10/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 527-2 |
Tisan TISAKRIL® 30% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Modulus of Elasticity | 5.50 GPa | 798 ksi | ISO 178 |
Addiplast Addilene J 326 V30 Polypropylene Copolymer High modulus, high durabilityInformation provided by Addiplast. |