Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.50 GPa | 363 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | DIN 53457 |
Ineos Nova S-3400 Medium Impact Compact Polystyrene
(discontinued **) Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. For injection molding generally a lubricated type is us.. |
|||
Modulus of Elasticity | 2.50 - 5.88 GPa | 363 - 853 ksi | Average value: 3.66 GPa Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1301-8148 PPS, linear, with PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1502-7867/BL4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 50-8479/BL-1 Polycarbonate, unreinforced Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia .. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 80-7014 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® NSB 90 NT Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 527 |
GEHR Plastics Corzan® PVC-C Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 527-2 |
Tisan TISAKRIL® Flame Retardant (V0) ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 15MM288 OPP Film Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. MM288 is designed for use as the center web of a triplex lamination. The treated surface offe.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 36MO747 OPP Film Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa .. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 527-1 |
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 178 |
Addiplast Addilene J 522 N30 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 527-2 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 178 |
Addiplast Addilene J 430 N30 Polypropylene Copolymer Good surface appearanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 178 |
Addiplast Addilene PMD 50284 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 527-2 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | 1 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Modulus of Elasticity | 2.50 - 11.87 GPa @Temperature -40.0 - 150 °C |
363 - 1722 ksi @Temperature -40.0 - 302 °F |
Average value: 5.80 GPa Grade Count:16 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Modulus of Elasticity | 2.50 - 3.80 GPa | 363 - 551 ksi | Average value: 3.12 GPa Grade Count:5 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Modulus of Elasticity | 2.50 GPa | 363 ksi | ISO 178 |
Addiplast Addilene H 462 M20 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |