Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.30 GPa | 334 ksi | ASTM D638 |
Plaskolite Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | dry |
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | 50% RH |
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ASTM D638 |
Plaskolite West Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Modulus of Elasticity | 2.30 - 2.75 GPa | 334 - 399 ksi | Average value: 2.41 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | DIN 53457 |
Ineos Nova S-5400 High Impact Compact Polystyrene
(discontinued **) Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding.. |
|||
Modulus of Elasticity | 2.30 - 4.83 GPa | 334 - 700 ksi | Average value: 3.30 GPa Grade Count:26 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 2.30 - 2.41 GPa | 334 - 350 ksi | Average value: 2.38 GPa Grade Count:6 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 2.30 - 27.6 GPa | 333 - 4000 ksi | Average value: 13.0 GPa Grade Count:13 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 50-7216 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 6-7833 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 80-7718 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | |
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 527-2 |
Tisan TISARBON® Flame Retardant (V0) Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Modulus of Elasticity | 2.30 - 4.30 GPa | 334 - 624 ksi | ASTM D638 |
Zeus PEEK Tubing PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 527-2 |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO R527 |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | Conditioned; ISO 178 |
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 178 |
Addiplast Addilene J 220 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 178 |
Addiplast Addilene J 520 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 178 |
Addiplast Addilene J 522 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 527-2 |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | DIN 53457 |
Ineos Nova S-3201 Medium Impact Compact Polystyrene
(discontinued **) Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to .. |
|||
Modulus of Elasticity | 2.30 GPa | 334 ksi | ISO 527 |
GEHR Plastics PPE Polyphenylene Ether
(discontinued **) Polyphenylenether belongs to the group of amorphous materials and can be used in temperatures ranging from -50°C to approximately 105°C. PPE exhibits a high impact strength, a low water absorption.. |