Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 207 MPa @Temperature 23.9 °C |
30000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D695 |
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle.. |
|||
Compressive Strength | 207 MPa | 30000 psi | |
Pyrotek TS-84 Thermoset Electrical Insulation Product (Nema Grade: XX) Paper reinforcement, Phenolic Resin, Natural/Black Color. Good insulation in dry or humid conditions.Information provided by Pyrotek. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Resinoid 1365 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Compressive Strength | 207 MPa | 30000 psi | |
Poco Graphite ZEE-2 Ion Implant Grade Graphite ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro.. |
|||
Compressive Strength | 207 MPa | 30000 psi | |
XX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
IDI Composites C-108 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
IDI Composites C-206 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
IDI Composites E-205 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Compressive Strength | 207 MPa @Thickness 12.7 mm |
30000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Haysite H900 Polyester, Glass Reinforced H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,.. |
|||
Compressive Strength | 207 MPa | 30000 psi | |
Haysite HCR-100 Corrosion Resistant Polyester/Glass Sheet A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray. |
|||
Compressive Strength | 207 MPa | 30000 psi | |
Haysite HCR-125 Corrosion Resistant Vinyl Ester/Glass Sheet A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix with flame retardant and ultraviolet inhibitors. Standard color is beige. Derakane® 470 is a registe.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 29502 Phenolic, Compression Grade Durez 29502 Brown Phenolic is a two stage, asbestos free, glass filled, special purpose molding material. It is formulated for close tolerance applications such as transmission valve bodies, and di.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Plenco 2308 Phenolic, Granular, Transfer Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Compressive Strength | 207 MPa | 30000 psi | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Compressive Strength | 207 MPa | 30000 psi | 1% offset; ASTM D695 |
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI) TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Compressive Strength | 207 MPa | 30000 psi | Lengthwise; ASTM D635 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 207 MPa | 30000 psi | Lengthwise; ASTM D635 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Compressive Strength | 207 MPa | 30000 psi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Compressive Strength | 207 MPa | 30000 psi | |
XXXPC Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.Information supplied by Sumitomo Bak North America. |