Pyrotek TS-84 Thermoset Electrical Insulation Product (Nema Grade: XX)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek TS-84 Thermoset Electrical Insulation Product (Nema Grade: XX).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Paper reinforcement, Phenolic Resin, Natural/Black Color. Good insulation in dry or humid conditions.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.346 g/cc
0.04863 lb/in³
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Flexural Strength 117 MPa
17000 psi
Compressive Strength 207 MPa
30000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 138 °C
280 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+11 ohm-cm
4.00e+11 ohm-cm
Dielectric Strength 20.0 kV/mm
508 kV/in