Material Notes:
Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrical and appliance applications. Shrinkage and mechanical strengths are closely controlled to meet part reliability requirements.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.4 g/cc
0.051 lb/in³
ASTM D792
Apparent Bulk Density 0.58 g/cc
0.021 lb/in³
ASTM D1895
Water Absorption 0.5 %
0.5 %
ASTM D570
Linear Mold Shrinkage 0.007 cm/cm
0.007 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55 MPa
8000 psi
ASTM D638
Tensile Modulus 9.6 GPa
1400 ksi
ASTM D638
Flexural Strength 76 MPa
11000 psi
Compressive Strength 207 MPa
30000 psi
ASTM D695
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
UL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 171 °C
340 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.0 mm
V-1

@Thickness 0.12 in
V-0

@Thickness 6.0 mm
V-0

@Thickness 0.24 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.0e+11 ohm-cm
1.0e+11 ohm-cm
ASTM D257
Dielectric Constant 4.7

@Frequency 1e+6 Hz
4.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.8 kV/mm
351 kV/in
Step by step; ASTM D149
15.7 kV/mm
399 kV/in
Short Time; ASTM D149
Dissipation Factor 0.05

@Frequency 1e+6 Hz
0.05

@Frequency 1e+6 Hz
ASTM D150