| Category | Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled |
| Manufacturer | Quantum Advanced Engineering Plastics |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quantum PEEK 30% Carbon Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
| Water Absorption | 0.10 % | 0.10 % | ASTM D570 |
| Water Absorption at Saturation | 0.30 % | 0.30 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 102 | 102 | ASTM D785 |
| Hardness, Rockwell R | 124 | 124 | ASTM D785 |
| Hardness, Shore D | 86 | 86 | ASTM 2240 |
| Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
| Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 7.58 GPa | 1100 ksi | ASTM D638 |
| Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
| Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
| Compressive Strength | 207 MPa | 30000 psi | ASTM D695 |
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
| Coefficient of Friction | 0.20 | 0.20 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.908 W/m-K | 6.30 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 340 °C | 644 °F | ASTM D3417 |
| Maximum Service Temperature, Air | 249 °C | 480 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 277 °C | 530 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | <= 1e+05 | <= 1e+05 | ASTM D257 |
| Dielectric Constant | 3.3 @Frequency 1.00e+6 Hz |
3.3 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 1.26 kV/mm | 32.0 kV/in | ASTM D149 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | no |