Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 200 MPa | 29000 psi | IPC 2.4.16 |
Rogers Corporation Ultralam® 3850 Liquid Crystalline Polymer Circuit Material ULTRALAM® 3850 laminate circuit materials utilize highly temperature resistant liquid crystalline polymer (LCP) as the dielectric film.Features & Benefits:Excellent high frequency propertiesStable .. |
|||
Tensile Strength | 200 MPa | 29000 psi | In Fiber direction +/- 45° to tensile axis; ASTM D3039 and D3518 |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Tensile Strength | 200 MPa | 29000 psi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Tensile Strength | 200 MPa | 29000 psi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |
|||
Tensile Strength | 200 MPa | 29000 psi | ASTM D638 |
Kuraray Genestar™ GN2450 Nylon, 45% Glass Filled High Strength V-0 Grade. Features a high strength and modulus. It is well suited for FPC sliders and IC sockets, as well as other components that require modulus and dimensional precision. |