Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Enduran 7062X PBT+PET (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC (Asia Pacific) LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific) 30% GR PBTP. Easy flow/release. High stiffness and load bearing properties.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0050 cm/cm @Thickness 2.30 - 4.60 mm |
0.0040 - 0.0050 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific) LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66 LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66 LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® HX420HP PBT Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific) LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0017 - 0.0050 cm/cm @Time 86400 sec |
0.0017 - 0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 LNP THERMOCOMP* PF006S is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |