Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 265 °C |
12 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 330 °C |
12 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 330 °C |
12 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 330 °C |
12 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 330 °C |
12 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 280 °C |
12 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 340 °C |
12 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East) Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 340 °C |
12 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 265 °C |
12 g/10 min @Load 2.65 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 265 °C |
12 g/10 min @Load 2.65 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
12 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 340 °C |
12 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
Typical |
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 280 °C |
12 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 280 °C |
12 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 280 °C |
12 g/10 min @Load 2.65 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 330 °C |
12 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |