Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition B; ASTM D1693 |
NOVA Chemicals Novapol® HB-W646-U HDPE Blow Molding Resin Features: High molecular weight HDPEExcellent ESCRImpact strengthGood processability Applications: DrumsJerry cansIBCsMarine fuel tanksInformation provided by Nova Chemicals |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50, condition B; ASTM D1693 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Bent Strip, Condition A & B, F50 values, From compression molded samples; ASTM D 1693 |
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693 |
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Thickness 3.18 mm |
>= 1000 hour @Thickness 0.125 in |
bent strip, non slit; ASTM D1693 |
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin
(discontinued **) MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Conditions A and B; ASTM D1693 |
Chevron Phillips Marlex® C516 HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Outstanding impact resistanceOutstanding creep resistanceExcellent ESCRExcellent chemical resistanceExcellent melt stabilityApplications: 55 gallon drums.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of go.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A; ASTM D1693 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A; ASTM D1693 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applica.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D-1693 |
Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applica.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1963A |
ExxonMobil HDPE HD 9856B High Density Polyethylene Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil LL 8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LLP 8360.29 Linear Low Density Polyethylene Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
ESCR 100% Igepal® | 1000 hour @Temperature 50.0 °C |
1000 hour @Temperature 122 °F |
ASTM D1693 B |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem GP5550 HDPE High Density Extrusion Polyethylene GP5550 is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. Its applications .. |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil LL 8360 Rotational Molding Resin
(discontinued **) LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha.. |
|||
ESCR 100% Igepal® | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
ASTM D1693 |
Unipetrol PE HD LITEN® VL 29 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
ESCR 100% Igepal® | >= 1000 hour | >= 1000 hour | Condition A, F50; ASTM D1693 |
Amco PRIMATOP HDPE 003946HP Blow Molding Polyethylene HDPE 003946HP features antistat, outstanding ESCR, and excellent impact resistance. Applications include detergent bottles, industrial containers, large parts, and household and industrial chemical .. |