Material Notes:
GP5550 is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. Its applications include: straight pipes for mining, subducts for energy and telecom, jacketing of optic fibers and metallic cables, geomembranes, and blends for irrigation pipes.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM-D792
ESCR 100% Igepal® >= 1000 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 0.23 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.23 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM-D2240
Tensile Strength at Break 38.0 MPa
5510 psi
ASTM-D638
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM-D638
Elongation at Break 780 %
780 %
ASTM-D882
Elongation at Yield 8.4 %
8.4 %
ASTM-D882
Flexural Modulus, 1% Secant 1150 MPa
167000 psi
ASTM-D790
Izod Impact, Notched 3.40 J/cm
6.37 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
ASTM-D648
Vicat Softening Point 125 °C

@Load 1.02 kg
257 °F

@Load 2.25 lb
ASTM-D1525