A. Schulman LP544-01 High-Density Copolymer Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Copolymer Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman LP544-01 High-Density Copolymer Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermoformed parts and profile extrusions. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.946 g/cc
0.946 g/cc
ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A; ASTM D1693
Melt Index of Compound 0.25 g/10 min

@Temperature 190 °C
0.25 g/10 min

@Temperature 374 °F
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Yield 22.1 MPa
3200 psi
2"/min; ASTM D638
Elongation at Break >= 700 %
>= 700 %
2"/min; ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C
150 °F
ASTM D648