Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Melt Flow | 0.20 g/10 min @Load 1.00 kg, Temperature 235 °C |
0.20 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 5300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.20 g/10 min @Load 1.00 kg, Temperature 235 °C |
0.20 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 5500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.20 - 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4850B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.20 - 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4851B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.20 - 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.20 - 0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 0.20 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.20 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 0.20 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.20 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Melt Flow | 0.20 - 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®. |
|||
Melt Flow | 0.20 - 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Forever Plast Namtene® Recycled Standard HDPE Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 250 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 250 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Melt Flow | 0.20 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.20 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8006 Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB/FL 20 HDPE Made for tubular film and special applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® SB/SL 20 HDPE Made for blow molding, tubular film and special applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg |
0.20 g/10 min @Load 4.76 lb |
ISO 1133 |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg |
0.20 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133/D |
Total MDPE 3802 B Medium Density Polyethylene, Cable MDPE 3802 B is a black medium density polyethylene particularly suited for cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium and high .. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133/D |
Total MDPE 3802 Medium Density Polyethylene, Cable MDPE 3802 is a natural medium density polyethylene particularly suited for colored cable sheathing applications and designed to meet the requirements for telecommunication and power cables (medium a.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Melt Flow | 0.20 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.20 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ASA 5946 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.20 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.20 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ASA S-150E-1115 ASA Weatherable Polymers Extrusion Grade, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T10 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F60 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg |
0.20 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lacqtene® 2002 TN 40 HDPE, blow molding, pipe, sheet
(discontinued **) LACQTENE® 2002 TN 40 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer.Information provided provided by Total Petrochemicals.Total Petrochemic.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg |
0.20 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lacqtene® 6002 FLG 42 HDPE film
(discontinued **) LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h.. |
|||
Melt Flow | 0.20 g/10 min @Load 2.16 kg |
0.20 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lacqtene® 2001 TBK 40 HDPE pipe
(discontinued **) LACQTENE® 2002 TBK 40 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2002 TBK 40 is a black compound especially developed for.. |