Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASA S-150E-1115 ASA Weatherable Polymers Extrusion Grade, Medium Impact

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA S-150E-1115 ASA Weatherable Polymers Extrusion Grade, Medium Impact.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 0.20 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.20 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
3.9 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.9 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 50.3 MPa
7300 psi
chs 2.0 in/min; ASTM D638
Flexural Strength 57.8 MPa
8380 psi
tangent; chs 0.05 in/min; ASTM D790
Flexural Modulus 2.308 GPa
334.7 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 2.67 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
5.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C

@Load 1.00 kg,
Thickness 3.17 mm
198 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525