Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Breplast Bretene TS COR Plus High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Breplast S.P.A.
Trade Name Bretene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Breplast Bretene TS COR Plus High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Recovered polyethylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Density >= 0.950 g/cc
>= 0.0343 lb/in³
UNI EN ISO 1183-1
Melt Flow 0.20 - 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 - 0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
UNI EN ISO 1133
1.0 - 1.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.0 - 1.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
UNI EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527-1-2
Elongation at Break 550 %
550 %
ISO 527
Descriptive Properties Value Comments
Color Grey / Green
Users viewing this material also viewed the following: