Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® FR30U ABS Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® G320 ABS (Europe-Africa-Middle East) CYCOLAC G320 is a super high impact resistant ABS grade. It combines impact resistance with high stiffness, good temperature resistance and processability. It has a good fit in automotive interiors .. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1295 PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 200 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXD951A PC Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | >= 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
>= 7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
MTM Plastics Dipolen® SP Recycled PP Blend Dipolen® SP is a granulated polypropylene with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to custo.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC0703 PC PC0703 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC0703R PC PC0703R resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.This data was supplied by SABIC-IP f.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS 1000 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Chi Mei Kibiton® PB-585 SBC Shoe sole industrial accessory |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |