Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.0 - 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Melt Flow | 1.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
1.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 1.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
1.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Melt Flow | 1.0 - 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.0 - 3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) HB5020 High Density Polyethylene HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 1.0 g/10 min @Load 10.0 kg, Temperature 200 °C |
1.0 g/10 min @Load 22.0 lb, Temperature 392 °F |
ISO 1133 |
Kuraray SEPTON® S1001 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg |
1.0 g/10 min @Load 11.0 lb |
ISO 1133 |
SIDPEC EGYPTENE® HD 5402 EA HDPE Pipe Grade Applications:Ducting pipeDrainage PipeNon-pressure pipeInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BL2571 High Density Polyethylene BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB/FL 20 HDPE Made for tubular film and special applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® SB/SL 20 HDPE Made for blow molding, tubular film and special applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil PP7011L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets .. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 4001H3F Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 4001HH Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABSPC 8901P ABS/PC Plating Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TW-18B1 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.0 g/10 min @Load 1.05 kg, Temperature 190 °C |
1.0 g/10 min @Load 2.31 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS/PC 8901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T10 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR Plus T15 High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 1.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS COR White F High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 1.0 - 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |