Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
5.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
17.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
17.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.8 MPa
6640 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.336 GPa
338.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.015 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.902 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C

@Load 1.00 kg,
Thickness 3.17 mm
221 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525