Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 381 - 12700 microns | 15.0 - 500 mil | Range of Standard Thicknesses |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Thickness | 381 - 12700 microns | 15.0 - 500 mil | Range of Standard Thicknesses |
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Thickness | 381 microns | 15.0 mil | per ply, 8HS form |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, ENKA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Thickness | >= 381 microns | >= 15.0 mil | DC |
Parker Chomerics CHO-BOND 4660 Conductive Caulk/Sealant CHO-BOND® 4660 caulking compound is a single-component, electrically conductive, paste-like material intended for EMI shielding and grounding applications. Its non-hardening characteristic makes it.. |
|||
Thickness | 381 microns | 15.0 mil | |
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Thickness | 381 microns | 15.0 mil | 1564 Fiberglass, Substrate |
Arlon R3313X016-38 0.0165" (0.419 mm) Cured Silicone Rubber with Fiberglass Substrate 38" Wide
(dis Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 380 microns | 15.0 mil | Standard |
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu.. |
|||
Thickness | 381 microns | 15.0 mil | |
Zircar Zirconia ZYW-15 Zirconia Cloth Insulation Zirconia Cloths Type ZYW are flexible textiles composed of yttria stabilized zirconia fibers that offer extreme temperature and chemical resistance in a flexible form. Type ZYW cloths provide the lo.. |
|||
Thickness | 381 microns | 15.0 mil | Total; ASTM D3652 |
3M 2552/Silver Damping Foils General purpose vibration dampingInformation provided by 3M |
|||
Thickness | 381 microns | 15.0 mil | Rubber |
Arlon 30570R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Thickness | 381 microns | 15.0 mil | Silicone |
Arlon 41580R015 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Thickness | 381 microns | 15.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Thickness | 381 microns | 15.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51981XA015 0.0150" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil PolyethyleneThis data r.. |
|||
Thickness | 381 microns | 15.0 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R35551X015 0.015" Uncured Silicone Rubber with Woven Fabric Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Primed 3M Nextel 312 Woven Fabric AF-10, HCSide 2: Uncured Silicone RubberThis data represents typica.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |
|||
Thickness | 381 microns | 15.0 mil | Tape |
3M 412DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51149R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassLayer 1: Cured Silicone RubberThis data represents typical values for the production mat.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51268R015P 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data r.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 915-10R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |
|||
Thickness | 381 microns | 15.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber 2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part num.. |
|||
Thickness | 381 microns | 15.0 mil | Rubber |
Arlon R30370A015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Thickness | 381 microns | 15.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon T3015-R004 0.015" (0.381 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Thickness | 381 microns | 15.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 31560R015 0.015" (0.381 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE Carrier This data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 381 microns | 15.0 mil | Side 1 |
Arlon 44602W020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone rubber on fiberglassThis data represents typical values for the production material.. |
|||
Thickness | 381 microns | 15.0 mil | overall; Arlon SQA-TMS-003 |
Arlon R37881R015 Silicone Rubber/Fiberglass Interleave: 1.5 mil PE; Side 1: uncured silicone rubber; Substrate: 1528 fiberglass; Side 2: uncured silicone rubber; Interleave: 1.5 mil PE |
|||
Thickness | 381 microns | 15.0 mil | overall; Arlon SQA-TMS-003 |
Arlon R37908R015L Silicone Rubber/Fiberglass/Acrylic/Polyester Laminated film: aluminized PEN; Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2, layer 1: acrylic PSA; Side 2, layer 2: polyester substrate; Side 2, layer 3: acrylic PSA; Interleav.. |