GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material

Category Carbon , Graphite
Manufacturer GrafTech International
Trade Name GRAFOIL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous purity specifications of the nuclear industry, including the General Electric Nuclear Nonmetallic Material Specification D50YP12 (Rev 2) and is typically 99.8% graphite. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced.
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
Thickness 250 microns
9.84 mil
Standard
380 microns
15.0 mil
Standard
760 microns
29.9 mil
Standard
Ash 0.50 %
0.50 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 525 °C
977 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.0015 %
0.0015 %
Carbon, C 99.5 %
99.5 %
Copper, Cu <= 0.0010 %
<= 0.0010 %
Mercury, Hg <= 0.000050 %
<= 0.000050 %
Phosphorous, P 0.050 %
0.050 %
Sulfur, S 0.045 %
0.045 %
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) <= 10 ppm
<= 10 ppm
Leachable
Descriptive Properties Value Comments
Total Chlorides (%) <50
Total Fluorides (ppm) <50
Total Halogens (ppm) 40
Total Nitrates (ppm) 10
Total Nitrites (ppm) 1