Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 25.0 microns | 0.984 mil | |
SABIC F04660 High Density Polyethylene for Blown Film Applications Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp.. |
|||
Thickness | >= 25.0 microns | >= 0.984 mil | |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
Thickness | 25.0 microns | 0.984 mil | As tested for properties on this data sheet |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Total Finathene® LL 6010 FH 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Formosa Plastics Formolene® FORMAX® L71709E2 Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
Thickness | 25.0 microns | 0.984 mil | extruded at 2.5:1 BUR |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
Thickness | 25.0 microns | 0.984 mil | ASTM D374 |
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
(discontinued * VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t.. |
|||
Thickness | >= 25.0 microns | >= 0.984 mil | |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Thickness | >= 25.0 microns | >= 0.984 mil | |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin Features: Excellent processabilityGood stiffness and strengthHigh stretchability Applications: Overwrap filmNettingBlend resinInformation provided by Nova Chemicals |
|||
Thickness | 25.0 - 75.0 microns | 0.984 - 2.95 mil | Recommended range for processing |
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem Flexus® 9210 LLDPE Blown Film Extrusion
(discontinued **) 25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 25 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Thickness | 25.0 microns | 0.984 mil | As Tested |
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU) Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU .. |
|||
Thickness | 25.0 microns | 0.984 mil | As Tested |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Thickness | 25.0 microns | 0.984 mil | Minimum recommended |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Thickness | 25.0 - 300 microns | 0.984 - 11.8 mil | possible range, depending on extrusion conditions |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4701 copolymer is an ultra low density polyethylene having high pinhole and puncture resistance, tear strength and high impact resistance combined with improved softness. It has low levels .. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem Flexus® 9200 LLDPE Blown Film Extrusion Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing .. |
|||
Thickness | 25.0 - 150 microns | 0.984 - 5.91 mil | Average value: 54.3 microns Grade Count:24 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Thickness | 25.0 - 150 microns | 0.984 - 5.91 mil | possible range, depending on extrusion conditions |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade DOW LDPE 607A resin is a fully formulated high clarity blown film resin for thin gauge optical applications, such as bakery film. It contains medium levels of slip additive and low levels of antiblo.. |