Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® LL 6010 FH 18P LLDPE film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® LL 6010 FH 18P LLDPE film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
on fluff; ISO 1183
Thickness 25.0 microns
0.984 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ISO 527
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO 527
Film Elongation at Break, MD 600 %
600 %
ISO 527
Film Elongation at Break, TD 750 %
750 %
ISO 527
Secant Modulus, MD 0.180 GPa
26.1 ksi
ISO 5527
Secant Modulus, TD 0.200 GPa
29.0 ksi
ISO 5527
Dart Drop Test 170 g
0.375 lb
25µ; ISO 7765-1
Film Tensile Strength at Break, MD 45.0 MPa
6530 psi
ISO 527
Film Tensile Strength at Break, TD 40.0 MPa
5800 psi
ISO 527
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
ISO 11357-3
Optical Properties Metric English Comments
Haze 14 %
14 %
25µ; ASTM D 1003
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.
Users viewing this material also viewed the following: