Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DOW LDPE 607A resin is a fully formulated high clarity blown film resin for thin gauge optical applications, such as bakery film. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
Thickness 25.0 microns
0.984 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg
2.0 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.1 MPa
1750 psi
Film Tensile Strength at Yield, TD 12.0 MPa
1740 psi
Coefficient of Friction 0.20
0.20
Elmendorf Tear Strength MD 300 g
300 g
Elmendorf Tear Strength TD 250 g
250 g
Elmendorf Tear Strength, MD 12.0 g/micron
305 g/mil
Elmendorf Tear Strength, TD 10.0 g/micron
254 g/mil
Optical Properties Metric English Comments
Haze 3.8 %
3.8 %
Gloss 77 %
77 %
45°
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Processing Temperature 188 °C
370 °F
Film extrusion temperature