Physical Properties Metric English Comments
Melt Flow 45 g/10 min
45 g/10 min
I<sub>21</sub>; ASTM D238
Petromont 8001 High Density Polyethylene Resin
Pétromont HDPE 8001 is a high density, homopolymer polyethylene resin produced using the UNIPOL® Process. This high strength resin is intended for extrusion on cast line, where excellent processab..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
SABIC PP 6711K Polypropylene Copolymer for Injection Molding
Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro..
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 380 °C
45 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Kingfa LONOY 1200 PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical LUCEL N145LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer
INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 320 °C
45 g/10 min

@Load 4.76 lb,
Temperature 608 °F
ASTM D1238
Kuraray Genestarâ„¢ G1300H Nylon, 30% Glass Filled
Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in ..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 300 °C
45 g/10 min

@Load 11.0 lb,
Temperature 572 °F
Lehmann & Voss LUVOCOM® 50/TF/15/BK Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Techmer ES Plastiblend® PC/ASA FR1508 UV
Availability: North AmericaForms: PelletsAdditive: Flame Retardant and UV StabilizerFeatures: Flame Retardant, Good UV Resistance and Halogen FreeInformation provided by TP Composites, Inc.
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 250 °C
45 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® AR-9301 PA, Glass Filled General Purpose
Information provided by Samsung Cheil Industries.
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 250 °C
45 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 265 °C
45 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis BH980MO Polypropylene Copolymer
BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer
Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis BorPURE™ RJ377MO Polypropylene, Transparent Random Copolymer
BorPure™ RJ377MO is a specially modified high MFR transparent polypropylene random copolymer based on proprietary Borealis Nucleation Technology (BNT), with an excellent organoleptic performance. N..
Melt Flow 45 - 65 g/10 min

@Load 8.70 kg,
Temperature 190 °C
45 - 65 g/10 min

@Load 19.2 lb,
Temperature 374 °F
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane
Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 160 °C
45 g/10 min

@Load 4.76 lb,
Temperature 320 °F
cm<sup>3</sup>/10 min; ISO 1133
EMS-Griltech Griltex® D 1260 A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melt Flow 45 g/10 min
45 g/10 min
ASTM D1238
ExxonMobil Escorene™ UL 04533EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 04533EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Fre..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 260 °C
45 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 275 °C
45 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su..
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 260 °C
45 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade
(PBT+X)-MD40Information provided by BARLOG plastics GmbH.
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 220 °C
45 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 220 °C
45 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Braskem CP 144 Coating Polypropylene
Information provided by Braskem
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Braskem CP 145 Injection Molding Polypropylene
Applications: Household; thin-walled parts; easy mould filling. Information provided by Braskem
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Braskem H 117 Injection Molding Polypropylene
Description: H 117 is a ultra-high melt flow rate homopolymer. This product is suitable to high productivity on thin-walled parts. H 117 features an excellent stiffness, thermal resistance, low warp..
Melt Flow 45 g/10 min

@Load 5.00 kg,
Temperature 316 °C
45 g/10 min

@Load 11.0 lb,
Temperature 601 °F
Procedure B; ASTM D1283
Chevron Phillips Ryton® PR09 Polyphenylene Sulfide Resin  (discontinued **)
Off White Polyphenylene Sulfide ResinRyton® PR09 is a finely divided powder. Ryton® PPS exhibits excellent thermal stability and chemical resistance and is suitable for a variety of applications ..