Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® AR-9301 PA, Glass Filled General Purpose

Category Polymer , Thermoplastic , Nylon
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® AR-9301 PA, Glass Filled General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Melt Flow 45 g/10 min

@Load 10.0 kg,
Temperature 250 °C
45 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 157 MPa
22800 psi
5 mm/min; ASTM D638
Flexural Strength 216 MPa
31300 psi
2.8 mm/min; ASTM D790
Flexural Modulus 9.32 GPa
1350 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.686 J/cm

@Thickness 6.35 mm
1.29 ft-lb/in

@Thickness 0.250 in
ASTM D256
0.686 J/cm

@Thickness 3.17 mm
1.29 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 235 °C

@Thickness 6.40 mm
455 °F

@Thickness 0.252 in
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved