Material Notes:
BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antistatic/demolding additives. Components molded from this grade have excellent demolding properties, high stiffness and gloss, good impact strength and low taste and odor. Applications: containers and products with medium to long flow length, closures, House ware and packaging requiring high stiffness and good impact, articles with integral hinges and demands for high gloss, and products with thicker wall sections requiring short cycle time.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ISO 2309-2
Tensile Strength, Yield 34.0 MPa
4930 psi
50mm/min; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.75 GPa
254 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.250 J/cm²

@Temperature -20.0 °C
1.19 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 10.0 J

@Temperature 0.000 °C
7.38 ft-lb

@Temperature 32.0 °F
ISO 6603-2
10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high