Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC PP 6711K Polypropylene Copolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC PP 6711K Polypropylene Copolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow properties & better impact properties than homo PP counterparts. This grade contains advance clarifier & anti-static agent.PP 6711K has the following features:Consistent processabilityGood stiffnessExcellent clarityLow thicknessEasy to flowBetter cycle time when compared to normal random gradesLess energy consumptionTypical Applications: PP 6711K can be used mainly for clear, thin-wall containers, housewares, caps & closures and lids.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus, 1% Secant 1150 MPa
167000 psi
ASTM D790A
Izod Impact, Notched 0.560 J/cm
1.05 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 190 - 230 °C
374 - 446 °F
Barrel Temperature
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F
Copyright © lookpolymers.com All Rights Reserved