Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ N20 High Performance Polypropylene Nanocomposite Characteristics: Less shrinkage Solved distortion problem Good balance in impact and stiffness High gloss Reduce production cycleApplications: Household Industry Electrical Appliances Toys Industry .. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 11-3225 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Melt Flow | 32 g/10 min @Load 5.00 kg, Temperature 200 °C |
32 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000 PC Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylex® P1032L Polycarbonate, Unreinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen EP640R Injection Molding Grade Polypropylene Moplen EP640R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640R is a block copolymer particularly suitable for injection.. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen EP540R Injection Molding Grade Polypropylene Moplen EP540R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540R is a block copolymer particularly suitable for injection.. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 260 °C |
32 g/10 min @Load 22.0 lb, Temperature 500 °F |
ASTM D1238 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Melt Flow | 32 g/10 min @Load 5.00 kg, Temperature 275 °C |
32 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Flow | 32 - 38 g/10 min @Load 2.16 kg, Temperature 235 °C |
32 - 38 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 32 g/10 min @Load 5.00 kg, Temperature 260 °C |
32 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® B 30 S FN40 000000 Nylon 6 PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 300 °C |
32 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 250 °C |
32 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Silon Tabond 5009 Adhesive Resin Tabond 5009 is a chemically modified Polypropylene. This grade is for coextrusion coating of multilayer film to give adhesion between the layers.Characteristics: • Strong adhesion to Aluminium .. |
|||
Melt Flow | 32 g/10 min @Load 1.20 kg, Temperature 224 °C |
32 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 230 °C |
32 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 190 °C |
32 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Melt Flow | 32 - 37 g/10 min @Load 5.00 kg, Temperature 372 °C |
32 - 37 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Melt Flow | 32 g/10 min | 32 g/10 min | Condition not noted.; ASTM D1238 |
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Melt Flow | 32 g/10 min @Load 10.0 kg, Temperature 220 °C |
32 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Melt Flow | 32 g/10 min @Load 2.16 kg, Temperature 280 °C |
32 g/10 min @Load 4.76 lb, Temperature 536 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber
(discontinued **) PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability |