Material Notes:
Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D792
Melt Flow 32 g/10 min

@Load 2.16 kg,
Temperature 190 °C
32 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58
52 - 58
Instantaneous; ASTM D2240
Tensile Strength at Break 7.93 MPa
1150 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 0.345 GPa
50.0 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), 1 % Secant; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature -76.1 °C
-105 °F
ASTM D746