Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.9 g/10 min | 3.9 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 8592 MEDIUM TAUPE Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Melt Flow | 3.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 2185 R15 Polyamide + PP Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho.. |
|||
Melt Flow | 3.9 g/10 min @Load 21.6 kg, Temperature 150 °C |
3.9 g/10 min @Load 47.6 lb, Temperature 302 °F |
Internal Method |
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Melt Flow | 3.9 g/10 min @Load 2.16 kg, Temperature 210 °C |
3.9 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Melt Flow | 3.9 g/10 min | 3.9 g/10 min | (Condition I) ASTM D-1238-94a |
Multibase Multi-ABS 8933 Black Ash is 28% per ASTM D-5630-94.Data provided by Multibase. |
|||
Melt Flow | 3.9 g/10 min | 3.9 g/10 min | ISO 1133 |
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Melt Flow | 3.9 g/10 min @Load 10.0 kg, Temperature 250 °C |
3.9 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Spartech Royalite R60M Hi-Impact ABS/PVC Resin Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are air.. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Spartech Royalite R61M Low Smoke Resin Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage.. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HR-1360 HIPS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HR-1360 HIPS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 3.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borclean™ HC314BF Polypropylene Homopolymer for Capacitor Film Borclean HC314BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC314BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 3.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem ML4400N LLDPE Rotomolding Polyethylene The resin ML4400N is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long t.. |
|||
Melt Flow | 3.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2640 E4 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 421 High Impact Polystyrene Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf.. |
|||
Melt Flow | 3.9 g/10 min | 3.9 g/10 min | ISO 1133 |
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |
|||
Melt Flow | 3.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ AG700 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |