Multibase Multi-ABS 8933 Black

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Multibase
Trade Name Multi-ABS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 8933 Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ash is 28% per ASTM D-5630-94.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0024 cm/cm
0.0024 in/in
ASTM D955-89
Melt Flow 3.9 g/10 min
3.9 g/10 min
(Condition I) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.3 MPa
6280 psi
ASTM D638-95
Elongation at Break 16.3 %
16.3 %
ASTM D638-95
Flexural Strength 65.5 MPa
9500 psi
ASTM D790-95
Flexural Modulus 5.903 GPa
856.2 ksi
RT; ASTM D-790-95
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256-93a