Material Notes:
Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 3.9 g/10 min
3.9 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
10 sec; ASTM D-2240
Tensile Strength, Ultimate 14.0 MPa
2030 psi
ASTM D638
Elongation at Break 725 %
725 %
ASTM D638
Flexural Strength 2.60 MPa
377 psi
1% Sec; ASTM D-790-92
Flexural Modulus 0.0779 GPa
11.3 ksi
1% Sec; ASTM D-790-92
Tear Strength 64.8 kN/m
370 pli
ASTM D624